Thermanit 18/17 E Mn
Solid wire, high-alloyed, stainless
Classifications
EN ISO 14343-A | G Z 18 16 5 N L |
---|---|
AWS A5.9 | ER317L(mod.) |
Mat. No. | 1.4453 |
Approvals
TÜV CECharacteristics
Stainless; resistant to intercrystalline corrosion and wet corrosion up to 400 °C (752 °F). High Mo content provides elevated resistance to Cl-bearing environment and pitting corrosion. Non magnetic. Well suited for joining and surfacing to matching and similar austenitic non-stabilized and stabilized stainless and non magnetic CrNiMo(N) steels / cast steel grades. Recommended for joining matching/similar austenitic and ferritic steels / cast steel grades with a maximum application temperature of 300 °C (572 °F). Well suited for depositing intermediate layers when welding products clad with a matching or similar overlay.
Dimensions
ø (mm) | Spool |
---|---|
1.0 | B300 |
1.2 | B300 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.