Thermanit 19/15
Solid wire, high-alloyed, stainless
Classifications
EN ISO 14343-A | G 20 16 3 Mn N L |
---|---|
AWS A5.9 | ER316LMn |
Mat. No. | 1.4455 |
Approvals
TÜV DB CECharacteristics
Stainless; resistant to intercrystalline corrosion and wet corrosion up to 350 °C (662 °F). Corrosionresistant similar to low-carbon CrNiMoMn(N) steels / cast steel grades. Seawater resistant, good resistance to nitric acid; Non magnetic (permeability in field of 8000 A/m 1.01 max.). Particularly suited for corrosion conditions in urea synthesis plants; well suited for joining and surfacing applications with matching and similar austenitic CrNi(N) and CrNiMo(Mn,N) steels/cast steel grades.
Dimensions
ø (mm) | Spool |
---|---|
1.0 | B300 |
1.2 | B300 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.