Thermanit 25/09 CuT
Solid wire, high-alloyed, stainless
Classifications
| EN ISO 14343-A | G 25 9 4 N L |
|---|---|
| AWS A5.9 | ER2594 |
| Mat. No. | ≈1.4501 |
Approvals
no approvalsCharacteristics
Stainless; resistant to intercrystalline corrosion (Application temp.: –50 °C (–58 °F) up to 220 °C (48 °F). Very good resistance to pitting corrosion and stress corrosion cracking due to the high CrMo(N) content (pitting index ≥ 40). Well suited for the conditions in the offshore field.
Dimensions
| ø (mm) | Spool |
|---|---|
| 1.0 | B300 |
| 1.2 | B300 |
| 1.6 | B300 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.