Thermanit 25/14 E-309L Si

Solid wire, high-alloyed, stainless

Thermanit 25/14 E-309L Si

Classifications

EN ISO 14343-A G 23 12 L Si
AWS A5.9 ER309LSi
Mat. No. 1.4332

Approvals

TÜV CE GL

Download

Characteristics

Stainless. Well suited for depositing intermediate layers when welding cladded materials. Favorably high Cr and Ni contents, low C content. For joining unalloyed/low-alloy steels/cast steel grades or stainless heat resistant Cr steels / cast steel grades to austenitic steels / cast steel grades. For depositing intermediate layers when welding the side of plates clad with low-carbon – non stabilized or stabilized – austenitic CrNiMo(N) austenitic metals. Application temperature max. 300°C (572 °F).

Dimensions

ø (mm) Spool
0.8 BS300
1.0 B300
1.2 B300
1.6 B300