böhler welding by voestalpine

Thermanit 625

Solid wire, nickel-alloy

Thermanit 625

Classifications

EN ISO 18274 S Ni 6625 (NiCr22Mo9Nb)
AWS A5.14 ERNiCrMo-3
Mat. No. 2.4831

Approvals

TÜV DB CE

Download

Characteristics

High resistance to corrosive environment. Resistant to stress corrosion cracking. Resistant to scaling up to 1000 °C (1832 °F). Temperature limit: 500°C (932°F) max. in sulphureous atmospheres. High temperature resistant up to 900 °C (1652 °F). Good toughness at subzero temperatures as low as –196 °C (–321 °F). For joining and surfacing work with matching / similar corrosion-resistant materials as well as with matching and similar heat resistant, high temperature resistant steels and alloys. For joining and surfacing work on cryogenic austenitic CrNi(N)-steels / cast steel grades and on cryogenic Ni-steels suitable for quenching and tempering.

Dimensions

ø (mm) Spool
0.8 BS300
1.0 BS300
1.2 BS300
1.6 BS300

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.