Thermanit Nicro 82
Solid wire, nickel-alloy
Classifications
| EN ISO 18274 | S Ni 6082 (NiCr20Mn3Nb) |
|---|---|
| AWS A5.14 | ERNiCr-3 |
| Mat. No. | 2.4806 |
Approvals
TÜV CE GLCharacteristics
Nickel alloy; heat and high temperature resistant. Good toughness at subzero temperatures as low as –269 °C (–452 °F). Good for welding austenitic-ferritic joints. No Cr-carbide zone that become brittle in the ferrite weld deposit transition zone, even as a result of heat treatments above 300 °C (572 °F). Good for fabricating tough joints and surfacing with heat resistant Cr- and CrNi-steels and Ni-alloys. Temperature limits: 900 °C max. (1652 °F) for fully stressed welds. Resistant to scaling up to 1000 °C (1832 °F).
Dimensions
| ø (mm) | Spool |
|---|---|
| 0.8 | BS300 |
| 1.0 | BS300 |
| 1.2 | BS300 |
| 1.6 | BS300 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.