böhler welding by voestalpine

Thermanit X

Solid wire, high-alloyed, stainless

Thermanit X

Classifications

EN ISO 14343-A G 18 8 Mn
AWS A5.9 ER307(mod.)
Mat. No. 1.4370

Approvals

TÜV DB CE GL

Download

Characteristics

Stainless. Resistant to scaling up to 850 °C (1562 °F). No adequate resistance against sulphureous combustion gases at temperatures above 500 °C (932 °F). For joining and surfacing applications with heat resistant Cr-steels and heat resistant austenitic steels. Well suited for fabricating austenitic-ferritic joints - max. application temperature 300 °C (572 °F). For joining unalloyed/ low-alloy or Cr-steels to austenitic steels. Low heat input required in order to avoid brittle martensitic transition zones.

Dimensions

ø (mm) Spool
0.8 BS300
1.0 B300
1.2 B300
1.6 BS300