Thermanit 22/09

Stick electrode, high-alloyed, basic

Thermanit 22/09

Classifications

EN ISO 3581-A E 22 9 3 N L B 2 2
AWS A5.4 E2209-15
Mat. No. ≈1.4462

Approvals

TÜV CE

Download

Characteristics

Stainless; resistant to intercrystalline corrosion at max. application temperature 250 °C (482 °F). Good resistance to stress corrosion cracking in chlorine- and hydrogen sulphide bearing environments. High Cr and Mo contents provide resistance to pitting corrosion. For joining and surfacing work with matching and similar austenitc steels/cast steel grades. Attention must be paid to embrittlement susceptibility of the parent metal.

Dimensions

ø (mm) Length (mm)
2.5 350
3.2 350
4.0 350