Thermanit 25/09 CuT
Stick electrode, high-alloyed, stainless, basic

Classifications
EN ISO 3581-A | E 25 9 4 N L B 2 2 |
---|---|
AWS A5.4 | E2595-15 |
Mat. No. | ≈1.4501 |
Approvals
no approvalsCharacteristics
Stainless. Resistance to intercrystalline corrosion – wet corrosion up to 250 °C (482 °F). Very good resistance to pitting corrosion and stress corrosion cracking due to the high CrMo(N) content (pitting index > 40). Well suited for offshore applications.
Dimensions
ø (mm) | Length (mm) |
---|---|
2.5 | 300 |
3.2 | 350 |
4.0 | 350 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.