Thermanit 25/14 EW 309L-17

Stick electrode, high-alloyed, stainless, rutile

Thermanit 25/14 EW 309L-17

Classifications

EN ISO 3581-A E 23 12 L R 3 2
AWS A5.4 E309L-17
Mat. No. 1.4332

Approvals

TÜV CE GL CWB

Download

Characteristics

Well suited for fabricating austenitic/ferritic joints at max. application temperature 300 °C (572 °F). Stainless, wet corrosion up to 350 °C (662 °F). Suitable for depositing intermediate layers when welding clad products. For joining unalloyed / low alloy steels / cast steel grades or stainless/heat resistant Cr steels/cast steel grades to austenitic steels/cast steel grades. For depositing intermediate layers when welding the clad side of plates of low carbon, unstabilized or stabilized CrNi(Mo,N) austenitic metals.

Dimensions

ø (mm) Length (mm)
2.5 350
3.2 350
4.0 350
5.0 450

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.