böhler welding by voestalpine

Thermanit 625

Stick electrode, nickel-alloy, basic

Thermanit 625

Classifications

EN ISO 14172 E Ni 6625 (NiCr22Mo9Nb)
AWS A5.11 ENiCrMo-3
Mat. No. 2.4621

Approvals

TÜV CE GL

Download

Characteristics

High resistance to corrosive environments. Resistant to stress corrosion cracking. Resistant to scaling up to 1000 °C (1832 °F). Temperature limit: 500 °C (932 °F) max. in sulphureous atmospheres. High temperature resistant up to 900 °C (1652 °F). Good toughness at subzero temperatures as low as –196 °C (–321 °F). For joining and surfacing work with matching / similar corrosion resistant materials as well as on matching and similar heat resistant, high temperature steels and alloys. For joining and surfacing work with cryogenic austenitic CrNi(N) steels / cast steel grades and on cryogenic Ni steels suitable for quenching and tempering.

Dimensions

ø (mm) Length (mm)
2.5 250
3.2 300
4.0 350
5.0 400

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.