böhler welding by voestalpine

Thermanit Nicro 82

Stick electrode, nickel-alloy, basic

Thermanit Nicro 82

Classifications

EN ISO 14172 E Ni 6082 (NiCr20Mn3Nb)
AWS A5.11 ENiCrFe-3 (mod.)
Mat. No. 2.4648

Approvals

TÜV CE GL

Download

Characteristics

Stainless, heat resistant, high temperature resistant. Good toughness at subzero temperatures as low as –269 °C (–452 °F). Well suited for welding austenitic ferritic joints. No Cr-carbide zones that become brittle in the ferrite weld deposit transition zone, not even as a result of heat treatments above 300 °C (572 °F). Well suited for tough joints and surfacing on heat resistant Cr and CrNi steels and Ni-alloys. Temperature limits: 550 °C (122 °F) in sulphureous atmospheres, 900 °C max (1652 °F) for fully stressed welds. Resistant to scaling up to 1000 °C (1832 °F).

Dimensions

ø (mm) Length (mm)
2.5 300
3.2 300
4.0 350
5.0 400

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.