böhler welding by voestalpine

Thermanit 18/17 E Mn

TIG rods, high-alloyed, stainless

Thermanit 18/17 E Mn

Classifications

EN ISO 14343-A W Z 18 16 5 NL
AWS A5.9 ER317L(mod.)
Mat. No. 1.4453

Approvals

TÜV CE

Download

Characteristics

Stainless; resistant to intercrystalline corrosion and wet corrosion up to 400 °C (752 °F). High Mo content provides high resistance to Cl-bearing environment and pitting corrosion. Non magnetic. Well suited for joining and surfacing to matching and similar austenitic non-stabilized and stabilized stainless and non magnetic CrNiMo(N) steels / cast steel grades.

Dimensions

ø (mm) Length (mm)
1.0 1000
1.6 1000
2.0 1000
2.4 1000
3.2 1000

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.