böhler welding by voestalpine

Thermanit 25/09 CuT

TIG rods, high-alloyed, stainless

Thermanit 25/09 CuT

Classifications

EN ISO 14343-A W 25 9 4 N L
AWS A5.9 ER2594
Mat. No. ≈1.4501

Approvals

no approvals

Download

Characteristics

Super duplex stainless steel; resistant to inter-crystalline corrosion. Very good resistance to pitting corrosion and stress corrosion cracking due to the high CrMo(N) content (pitting index ≥40). Well suited for conditions in offshore application, particularly for welding of super-martensitic stainless steels (13 % Cr); extra low hydrogen in the filler material available on request. Service temperature: –50 °C to 220 °C (-58°F to 428 °F).

Dimensions

ø (mm) Length (mm)
1.6 1000
2.0 1000
2.4 1000
3.2 1000

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.