Thermanit 625
TIG rods, nickel-alloy

Classifications
EN ISO 18274 | S Ni 6625 (NiCr22Mo9Nb) |
---|---|
AWS A5.14 | ERNiCrMo-3 |
Mat. No. | 2.4831 |
Approvals
TÜV DB CECharacteristics
High resistance to corrosive environment. Resistant to stress corrosion cracking. Resistant to scaling up to 1000 °C (1832 °F). Temperature limit: 500°C (932 °F) max. in sulphureous atmospheres. High temperature resistant up to 900 °C (1652 °F). Good toughness at subzero temperatures as low as –196 °C (–321 °F). For joining and surfacing work with matching / similar corrosion-resistant materials as well as on matching and similar heat resistant, high temperature resistant steels and alloys. For joining and surfacing work on cryogenic austenitic CrNi(N) steels / cast steel grades and on cryogenic Ni-steels suitable for quenching and tempering.
Dimensions
ø (mm) | Length (mm) |
---|---|
1.6 | 1000 |
2.0 | 1000 |
2.4 | 1000 |
3.2 | 1000 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.