böhler welding by voestalpine

Thermanit Nicro 82

TIG rods, nickel-alloy

Thermanit Nicro 82

Classifications

EN ISO 18274 S Ni 6082 (NiCr20Mn3Nb)
AWS A5.14 ERNiCr-3
Mat. No. 2.4806

Approvals

TÜV DB CE GL

Download

Characteristics

Stainless; heat and high temperature resistant. Good toughness at subzero temperatures as low as –269 °C (–452 °F). Good for welding austenitic-ferritic joints. No Cr carbide zone that becomes brittle in the ferrite weld deposit transition zone, even as a result of heat treatments above 300 °C (572 °F). Good for fabricating tough joints and surfacing with heat resistant Cr- and CrNi- steels and Ni-alloys. Temperature limits: 900 °C max. (1652 °F) for fully stressed welds. Resistant to scaling up to 1000 °C (1832 °F).

Dimensions

ø (mm) Length (mm)
1.6 1000
2.0 1000
2.4 1000
3.2 1000

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.