Thermanit X

TIG rods, high-alloyed, stainless

Thermanit X

Classifications

EN ISO 14343-A W 18 8 Mn
AWS A5.9 ER307(mod.)
Mat. No. 1.4370

Approvals

TÜV DB CE

Download

Characteristics

Stainless. Resistant to scaling up to 850 °C (1562 °F). No adequate resistance against sulphureous combustion gases at temperatures above 500 °C (932 °F). For joining and surfacing applications with heat resistant Cr-steels / cast steel grades and heat resistant austenitic steels / cast steel grades. Well suited for fabricating austenitic-ferritic joints – max. application temperature 300 °C (572 °F). For joining unalloyed/low-alloy or Cr-steels / cast steel grades to austenitic steels. Low heat input required in order to avoid brittle martensitic.

Dimensions

ø (mm) Length (mm)
1.0 1000
1.6 1000
2.0 1000
2.4 1000
3.2 1000

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.