Thermanit 25/14 E-309L
TIG rods, high-alloyed, stainless

Classifications
EN ISO 14343-A | W 23 12 L |
---|---|
AWS A5.9 | ER309L |
Mat. No. | 1.4332 |
Approvals
TÜV CE GLCharacteristics
Stainless; wet corrosion up to 350 °C (662 °F). Well suited for depositing intermediate layers when welding cladded materials. Favourably high Cr- and Ni-contents, low C content. For joining unalloyed/low-alloy steels/cast steel grades or stainless heat resistant Cr-steels/cast steel grades to austenitic steels/cast steel grades. For depositing intermediate layers when welding the side of plates clad with low-carbon – non-stabilized and stabilized – austenitic CrNi(MoN) austenitic metals.
Dimensions
ø (mm) | Length (mm) |
---|---|
1.6 | 1000 |
2.0 | 1000 |
2.4 | 1000 |
3.2 | 1000 |
All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.