Thermanit H-347

TIG rods, high-alloyed, stainless

Thermanit H-347

Classifications

EN ISO 14343-A W 19 9 Nb
AWS A5.9 ER347
Mat. No. 1.4551

Approvals

TÜV DB CE

Download

Characteristics

Stainless; resistant to intercrystalline corrosion and wet corrosion up to 400 °C (752 °F). Corrosion-resistant similar to matching stabilized austenitic CrNi steels/cast steel grades. For joining and surfacing application with matching and similar – stabilized and non-stabilized – austenitic CrNi(N) steels and cast steel grades.

Dimensions

ø (mm) Length (mm)
1.0 1000
1.6 1000
2.0 1000
2.4 1000
3.2 1000

All information provided is based upon careful investigation and intensive research. However, we do not assume any liability for correctness and information is subject to change without notice.